AJ04 – Stress Corrosion Cracking of Control Arm Shafts – 2015 Porsche 918 Spyder

NHTSA Campaign Number: 18V287
Manufacturer PorscheeBay logo Cars North America, Inc.
Components SUSPENSION
Potential Number of Units Affected 305

 

Stress Corrosion Cracking of Control Arm Shafts

If the control arm connecting shafts crack, affecting vehicle handling, it can increase the risk of a crash.

 

Summary

PorscheeBay logo Cars North America, Inc. (PorscheeBay logo) is recalling certain 2015 PorscheeBay logo 918 Spyder vehicles. The connecting shafts of the longitudinal and transverse control arms may fail due to stress corrosion cracking, impacting vehicle handling.

 

Remedy

PorscheeBay logo will notify owners, and dealers will replace the longitudinal and transverse control arms, free of charge. The manufacturer has not yet provided a notification schedule. Owners may contact PorscheeBay logo customer service at 1-800-767-7243. PorscheeBay logo’s number for this recall is AJ04.

 

Notes

Owners may also contact the National Highway Traffic Safety Administration Vehicle Safety Hotline at 1-888-327-4236 (TTY 1-800-424-9153), or go to www.safercar.gov.

 

Check if your Porsche has a Recall

 


Manufacturer Reimbursement Plan

https://static.nhtsa.gov/odi/rcl/2018/RMRP-18V287-7216.pdf

 


Recall Acknowledgement

May 18, 2018

https://static.nhtsa.gov/odi/rcl/2018/RCAK-18V287-8835.pdf

 


 

SaleBestseller No. 1
Meguiar’s Ultimate Polish – High-Gloss Polish for a Show Car Shine – Permanently Removes Light Swirls to Produce a Deep, Wet Reflection with a High Gloss Shine - Easy to Use, 16 Oz
  • PREPS SURFACE: Pre-waxing glaze that prepares the surface for wax while offering deep reflections and high gloss.
  • BEST CAR GLOSS: Conditioning oils add depth of color and maximum gloss prior to waxing, especially on dark colored cars
  • REMOVE SWIRLS: Quickly and gently removes fine swirls and towel marks for mirror-like reflections
  • SAFE FOR CLEAR COATS: Safe and on all glossy paints, including clear coats
  • FLEXIBLE APPLICATION: Safe and effective by hand or dual action polisher like Meguiar's MT300 Dual Action Polisher
Bestseller No. 2
Meguiar's Ultimate Compound - Pro-Grade Car Scratch Remover, Paint Correction Compound that Removes Defects While Adding Gloss and Shine, Single Stage and Clear Coat Scratch Remove, 15.2 Oz
  • BUFF OUT IMPERFECTIONS: Meguiar's Ultimate Compound removes scratches, swirls & oxidation for a clear, perfect finish
  • SHOWROOM SHINE: Advanced car compound removes scratches, swirls, oxidation & water spots and restores color & clarity for a showroom shine in minutes
  • CLEAR COAT SAFE: Auto compound safely removes scratches and other defects without hazing on clear coats & all gloss paints. Easy DIY fix by hand or da polisher
  • LIKE-NEW SHINE: Meguiar's exclusive micro-abrasive technology quickly removes scratches & restores clarity and shine for a stunning, swirl-free finish.
  • FAST & FLAWLESS: Meguiar's Ultimate Compound cuts fast, removes scratches and swirls without hazing, leaving a pro-detailer finish.
SaleBestseller No. 3
Nu Finish The Once A Year Car Polish Liquid - 16 OZ
  • One 16 oz bottle of Nu Finish The Once A Year Car Polish
  • Automotive polish that is made up of a series of zinc cross-linking polymer emulsions that help it last longer than any other polish on the market
  • Nu Finish car polish can be applied anywhere, even in direct sunlight
  • Also an ideal boat polish, motorcycle polish and chrome polish
  • The only auto polish tough enough to be called "The Once A Year Car Polish”
SaleBestseller No. 4
Chemical Guys C4 & P4 Clear Cut Correction Compound and Precision Paint Perfection Polish Combo - Removes Scratches, Swirls, Towel Marks, and Etching, Restores Gloss, Polishing Kit - 2 x 16 oz
  • C4 & P4 PAINT CORRECTION COMBO (GAP40016) – Complete 2-step Chemical Guys polishing kit includes C4 Clear Cut Compound for removing defects and P4 Precision Polish for refining paint to a flawless high-gloss finish
  • REMOVES DEFECTS FAST – C4 Chemical Guys Clear Cut compound quickly cuts through scratches, swirls, oxidation, towel marks, and etching, restoring clarity and leveling paint for the polishing stage
  • PRECISION POLISHING POWER – P4 car polish refines paint after compounding, removing micro-marring and enhancing depth, gloss, and color vibrancy for a show-quality finish
  • SAFE FOR ALL PAINT TYPES – This car polishing kit works on clear coat, single-stage, and ceramic-coated vehicles; compatible with dual action, rotary, or hand application methods
  • PROFESSIONAL RESULTS AT HOME – This Chemical Guys kit delivers body shop–quality correction and shine in a user-friendly kit, perfect for enthusiasts and professional detailers alike
Bestseller No. 5
3D Speed All-In-One Polish & Wax – Scratch & Swirl Remover, Clear Coat Safe Paint Sealant – High Gloss Finish, Easy Application – 8oz – Made in USA
  • Correct & Protect In One Step: 3D Speed is the ultimate all-in-one car polish and wax. Its advanced formula cuts through light swirls, oxidation, and scratches while sealing the surface with a protective wax coat. Get correction and protection in a single application—no need for multiple products
  • Restore Color Depth & Gloss: Tired of dull, lifeless paint? Speed revives your paint’s original clarity and depth while delivering a wet, mirror-like gloss. Whether your ride is brand new or needs some love, SPEED brings out the best in your finish—leaving it smooth, vibrant, and protected
  • Fast Easy Application: Designed for speed and simplicity, this polish and wax goes on like butter and wipes off clean with no residue. Use it by hand for quick touch-ups or with a dual-action polisher for larger panels. It’s the ultimate time-saver for weekend warriors and pros alike
  • Effortless Scratch & Swirl Removal: Speed tackles minor surface imperfections like light scratches, swirl marks, and oxidation without aggressive compounding. Safe for clear coat finishes, it levels defects while protecting your paint—ideal for maintenance or prep before a show
  • Pro Grade Quality Made In The USA: Backed by over 25 years of detailing innovation, 3D Speed is proudly made in the USA and trusted by professional detailers worldwide. When you see “3D” on the bottle, you know what’s inside delivers real results—performance you can count on

Last update on 2026-05-28 / Affiliate links / Images from Amazon Product Advertising API


 

This product presentation was made with AAWP plugin.

Leave a Comment

Share to...